2507 Roestvrijstalen staaf
|
Specificaties van roestvrijstalen staaf |
|||
|
Gemeengoed |
Ronde staaf van roestvrij staal / platte staaf / hoekstaaf / vierkante staaf / kanaal |
||
|
Standaard |
AISI, ASTM, DIN, GB, JIS, SUS |
||
|
Materiaal |
301, 304, 304L, 309S, 321, 316, 316L, 317, 317L, 310S, 201.202.321, 329, 347, 347H 201, 202, 410, 420, 430, S20100, S20200, S30100, S30400, S30403, S30908, S31008 , S31600, S31635, enz. |
||
|
Certificering |
SGS, BV, enz |
||
|
Oppervlak |
Helder, gepolijst, soepel draaien (geschild), borstel, molen, gebeitst enz. |
||
|
Tijd om te bezorgen |
7-15 dagen na bevestiging van de bestelling. |
||
|
Handelstijd |
FOB, CIF, CFR |
||
|
Betaling |
T/T of L/C |
||
|
MOQ: |
1 ton |
||
|
Specificatie |
Item |
Maat |
Af hebben |
|
Ronde staaf van roestvrij staal |
19*3mm-140*12mm |
Zwart & gebeitst & helder |
|
|
Roestvrij stalen platte staaf |
19*3mm-200*20mm |
Zwart & gebeitst & helder |
|
|
Roestvrijstalen vierkante staaf |
Warmgewalst: S10-S40mm Koudgewalst: S5-S60mm |
Warmgewalst en gegloeid en gebeitst |
|
|
RVS hoekstaaf |
20*20*3/4mm-180*180*12/14/16/18mm |
Wit zuur en warmgewalst en gepolijst |
|
|
Roestvrij stalen kanaal |
6#, 8#, 10#, 12#, 14#, 16#, 18#, 20#, 22#, 24# |
Wit zuur en warmgewalst en gepolijst en gezandstraald |
|
|
Chemische eigenschappen van veelgebruikte austenitische materiaalkwaliteit van roestvrij staal |
|||||||||||
|
ASTM |
UNS |
NL |
JIS |
C% |
Mn% |
P% |
S% |
Si% |
Cr% |
Ni% |
Mo% |
|
201 |
S20100 |
1.4372 |
SUS201 |
≤0.15 |
5,5-7,5 |
≤0.06 |
≤0.03 |
≤1.00 |
16.00-18.00 |
3,5-5,5 |
- |
|
202 |
S202000 |
1.4373 |
SUS202 |
≤0.15 |
7,5-10,0 |
≤0.06 |
≤0.03 |
≤1.00 |
17.00-19.00 |
4.0-6.0 |
- |
|
301 |
S30100 |
1.4319 |
SUS301 |
≤0.15 |
≤2.00 |
≤0.045 |
≤0.03 |
≤1.00 |
16.00-18.00 |
6.0-8.0 |
- |
|
304 |
S30400 |
1.4301 |
SUS304 |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
18.00-20.00 |
8.0-10.5 |
- |
|
304L |
S30403 |
1.4306 |
SUS304L |
≤0.03 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
18.00-20.00 |
8,0-12,0 |
- |
|
309S |
S30908 |
1.4883 |
SUS309S |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
22.00-24.00 |
12,0-15,0 |
- |
|
310S |
S31008 |
1.4845 |
SUS310S |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤1,50 |
24.00-26.00 |
19,0-22,0 |
- |
|
316 |
S31600 |
1.4401 |
SUS316 |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
16.00-18.00 |
10.0-14.0 |
- |
|
316L |
S31603 |
1.4404 |
SUS316L |
≤0.03 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
16.00-18.00 |
10.0-14.0 |
2.0-3.0 |
|
317L |
S31703 |
1.4438 |
SUS317L |
≤0.03 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
18.00-20.00 |
11.0-15.0 |
2.0-3.0 |
|
321 |
S32100 |
1.4541 |
SUS321 |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
17.00-19.00 |
9,0-12,0 |
3.0-4.0 |
|
347 |
S34700 |
1.4550 |
SUS347 |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
17.00-19.00 |
9,0-13.0 |
- |
![]()
![]()
![]()
![]()
|
Verpakking: zeewaardige houten pallets, waterdicht papier, pvc-folie, tussenschotpapier, in 20 'of 40' container of volgens de eisen van de klant. |
|
-- 20ft GP: 5898mm (Lengte) x2352mm (Breedte) x2393mm (Hoog) |
|
-- 40ft GP: 12032mm (Lengte) x2352mm (Breedte) x2393mm (Hoog) |
|
-- 40ft HC: 12032mm (Lengte) x2352mm (Breedte) x2698mm (Hoog) |
![]()
![]()
Q1: Hoe zit het met de verzendkosten?
De verzendkosten zijn afhankelijk van veel factoren.Express zal het snelst zijn, maar het duurst.Zeevracht is ideaal voor grote hoeveelheden, maar langzamer.Neem contact met ons op voor specifieke verzendoffertes, die afhankelijk zijn van hoeveelheid, gewicht, modus en bestemming.
Vraag 2: Wat zijn uw prijzen?
Onze prijzen zijn onderhevig aan verandering afhankelijk van het aanbod en andere marktfactoren.We sturen u een bijgewerkte prijslijst nadat u contact met ons heeft opgenomen voor meer informatie.
Q3: Heeft u een minimale bestelhoeveelheid?
Ja, we hebben minimale bestellingen voor specifieke internationale producten, neem contact met ons op voor meer informatie.