2507 Batang baja tahan karat
|
Spesifikasi Batang Baja Tahan Karat |
|||
|
Komoditas |
Batang Bulat Stainless Steel/Bar Datar/Bar Sudut/Bar Persegi/Saluran |
||
|
Standar |
AISI, ASTM, DIN, GB, JIS, SUS |
||
|
Bahan |
301, 304, 304L, 309S, 321, 316, 316L, 317, 317L, 310S, 201,202,321, 329, 347, 347H 201, 202, 410, 420, 430, S20100, S20200, S30100, S30400, S30403, S30908, S31008 , S31600, S31635, dll. |
||
|
Sertifikasi |
SGS, BV, dll |
||
|
Permukaan |
Cerah, Dipoles, Belok halus (Kupas), Kuas, Penggilingan, Acar dll. |
||
|
Waktu pengiriman |
7-15 hari setelah konfirmasi pesanan. |
||
|
Waktu Perdagangan |
FOB, CIF, CFR |
||
|
Pembayaran |
T/T atau L/C |
||
|
MOQ |
1 Ton |
||
|
Spesifikasi |
Barang |
Ukuran |
Menyelesaikan |
|
Batang bulat baja tahan karat |
19*3mm-140*12mm |
Hitam & Acar & Cerah |
|
|
Batang datar baja tahan karat |
19*3mm-200*20mm |
Hitam & Acar & Cerah |
|
|
Batang persegi baja tahan karat |
Digulung panas: S10-S40mm Digulung dingin: S5-S60mm |
Gulungan panas & anil & acar |
|
|
Bilah sudut baja tahan karat |
20*20*3/4mm-180*180*12/14/16/18mm |
Asam putih & canai panas & Dipoles |
|
|
Saluran baja tahan karat |
6#, 8#, 10#, 12#, 14#, 16#, 18#, 20#, 22#, 24# |
Asam putih & canai panas & Dipoles & Sandblast |
|
|
Sifat Kimia Kelas Bahan Baja Tahan Karat Austenitik yang Sering Digunakan |
|||||||||||
|
ASTM |
UNS |
ID |
JIS |
C% |
M N% |
P% |
S% |
Si% |
Cr% |
Ni% |
bulan% |
|
201 |
S2010 |
1.4372 |
SUS201 |
0.15 |
5.5-7.5 |
0,06 |
0.03 |
1.00 |
16.00-18.00 |
3.5-5.5 |
- |
|
202 |
S2020 |
1.4373 |
SUS202 |
0.15 |
7.5-10.0 |
0,06 |
0.03 |
1.00 |
17.00-19.00 |
4.0-6.0 |
- |
|
301 |
S30100 |
1.4319 |
SUS301 |
0.15 |
2.00 |
0,045 |
0.03 |
1.00 |
16.00-18.00 |
6.0-8.0 |
- |
|
304 |
S30400 |
1.4301 |
SUS304 |
0,08 |
2.00 |
0,045 |
0.03 |
0.75 |
18.00-20.00 |
8.0-10.5 |
- |
|
304L |
S30403 |
1.4306 |
SUS304L |
0.03 |
2.00 |
0,045 |
0.03 |
0.75 |
18.00-20.00 |
8.0-12.0 |
- |
|
309S |
S30908 |
1.4883 |
SUS309S |
0,08 |
2.00 |
0,045 |
0.03 |
0.75 |
22.00-24.00 |
12.0-15.0 |
- |
|
310S |
S3108 |
1.4845 |
SUS310S |
0,08 |
2.00 |
0,045 |
0.03 |
1,50 |
24.00-26.00 |
19.0-22.0 |
- |
|
316 |
S31600 |
1.4401 |
SUS316 |
0,08 |
2.00 |
0,045 |
0.03 |
0.75 |
16.00-18.00 |
10.0-14.0 |
- |
|
316L |
S31603 |
1.4404 |
SUS316L |
0.03 |
2.00 |
0,045 |
0.03 |
0.75 |
16.00-18.00 |
10.0-14.0 |
2.0-3.0 |
|
317L |
S31703 |
1.4438 |
SUS317L |
0.03 |
2.00 |
0,045 |
0.03 |
0.75 |
18.00-20.00 |
11.0-15.0 |
2.0-3.0 |
|
321 |
S32100 |
1.4541 |
SUS321 |
0,08 |
2.00 |
0,045 |
0.03 |
0.75 |
17.00-19.00 |
9.0-12.0 |
3.0-4.0 |
|
347 |
S34700 |
1.4550 |
SUS347 |
0,08 |
2.00 |
0,045 |
0.03 |
0.75 |
17.00-19.00 |
9.0-13.0 |
- |
![]()
![]()
![]()
![]()
|
Packing: palet kayu layak laut, kertas tahan air, film pvc, kertas interleaving, dalam wadah 20 'atau 40' atau sesuai kebutuhan pelanggan. |
|
-- 20ft GP:5898mm(Panjang)x2352mm(Lebar)x2393mm(Tinggi) |
|
-- 40ft GP: 12032mm (Panjang) x2352mm (Lebar) x2393mm (Tinggi) |
|
--40ft HC:12032mm(Panjang)x2352mm(Lebar)x2698mm(Tinggi) |
![]()
![]()
Q1: Bagaimana dengan biaya pengiriman?
Biaya pengiriman akan tergantung pada banyak faktor.Express akan menjadi yang tercepat tetapi akan menjadi yang paling mahal.Angkutan laut sangat ideal untuk jumlah besar, tetapi lebih lambat.Silahkan hubungi kami untuk penawaran pengiriman tertentu, yang tergantung pada kuantitas, berat, mode dan tujuan.
Q2: Berapa harga Anda?
Harga kami dapat berubah tergantung pada pasokan dan faktor pasar lainnya.Kami akan mengirimkan daftar harga terbaru setelah Anda menghubungi kami untuk informasi lebih lanjut.
Q3: Apakah Anda memiliki jumlah pesanan minimum?
Ya, kami memiliki minimum order untuk produk internasional tertentu, silahkan hubungi kami untuk informasi lebih lanjut.